Acknowledgements & Reference papers for NSRP Flash Rust Project

Posted on 16. Mar, 2009 by .

0

Acknowledgments, Bibliography for NSRP Flash Rust Project These papers listed below are included for further reading with permission from JPCL, CleanerTimes, and Marine Log. All rights are retained by the publishers. Many people contributed to this module.  The technical team members include: National Shipbuilding Research Program SP-3 Panel, Todd Pacific Shipyard, Detyens Shipyard, Atlantic Marine […]

Continue Reading

Pressure Sensitive Tape Test for Quantity of Flash Rust

Posted on 16. Mar, 2009 by .

0

Pressure Sensitive Tape Test- for Quantity of Flash Rust- NSRP Project The Pressure Sensitive Tape Test described by Hempel is a modification of ISO 8502-3 (Pressure Sensitive Tape test for dust) and is not mentioned in VIS-4.  The tape test can be used as a permanent record.  If lint deposition is a concern, the project […]

Continue Reading

Summary of Major Points- Flash Rust Project NSRP

Summary of Major Points- Flash Rust Project NSRP

Posted on 16. Mar, 2009 by .

0

NSRP Flash Rust Project Metric Table, Control of Amount Summary of Major Points: 1.    Flash Rust is the rust that occurs from the time the waterjetting process starts to the time the water used for the waterjetting process dries. 2.    Control the quantity of Flash Rust by Project Planning           • During Removal Process           • As Water is drying […]

Continue Reading

Example of Pressure Wash on Moderate Flash Rust

Posted on 16. Mar, 2009 by .

1

Example of Pressure Wash on MFR: Below: the substrate is dry- but it is  darker (overall) than the original substrate. This surface is dry within 5 minutes. The standard pictures in VIS-4 do not provide these types of illustrations of pressure-washed surfaces. The upper half is not washed; the lower half has been pressure washed. […]

Continue Reading

Pressure Washing and Excess Flash Rust

Posted on 16. Mar, 2009 by .

0

What Happens if there is too much Flash Rust prior to painting?  Prior to the application of paint, the substrate must meet the procurement specifications.  Typical field remediation includes:  Pressure washing  Broom brushing  Blowing off with pressurized air  Solvent cloth or dry cloth wiping  Vacuum Upon polling contractors, it appears that pressure washing is the […]

Continue Reading

Summary of Wipe, Swatch, and Brush Methods

Posted on 15. Mar, 2009 by .

0

Core Idea: All Methods lead to the same conclusion.  None  Light  Moderate  Heavy Adopt the method with which you feel most comfortable and that is portable to different projects and sites.

Continue Reading

Summary of Brush Test

Posted on 15. Mar, 2009 by .

0

Summary- Brush Test:  Brushing flash rust is quick, simple, and very reproducible.  Adopt a standard brush and standard cloth.  Be consistent with one swipe and in the same direction and duration.  Practice brush strokes with even pressure  Keep the contact area consistent.  Cloth can be cut at the area of color transfer and placed in […]

Continue Reading

Different Areas with Brush Test

Posted on 15. Mar, 2009 by .

0

Comparative results: Heavy Flash Rust formed from water coming from holes. Different section where Light, moderate, and heavy flash rust had formed in close proximity.      

Continue Reading

Example of Moderate Flash Rust on Brush

Posted on 15. Mar, 2009 by .

0

Example of Moderate Flash Rust on Brush:

Continue Reading

Example of Brush Test on Light Flash Rust

Posted on 15. Mar, 2009 by .

0

Example of Brush Test on Light Flash Rust: This view has the sun Illuminating the surface.  Substrate appears darker as it is in shadow. Inspection is biased by lighting angle.